Final surface of the milled testpat with a initial bulk of material of 5 mm at 24.000 rpm: Mean roughness Ra in microns and detail of the marks. |
|||||||
---|---|---|---|---|---|---|---|
![]() ![]() |
Description
Final surface of the milled testpat with a initial bulk of material of 5 mm at 24.000 rpm: Mean roughness Ra in microns and detail of the marks. |
||||||